Mn13 high manganese steel hardness : its surface hardness from HB200 quickly lifted to more than HB500, This results in a high abrasion resistant surface layer, while the steel plate inner austenite s
Mn13 is non-magnetic steel ,its Carbon content minimum data is 1% ,Mn content minimun data is 11% ;Its surface hardness from HB200 quickly lifted to more than HB500 while it works .
Mn13 is non-magnetic steel ,its Carbon content minimum data is 1% ,Mn content minimun data is11%,Its surface hardness from HB200 quickly lifted to more than HB500 while it works .
Due to Mn is the forming elements of net carbide, when cutting temperature higher than 350 ℃, along the cutting edge of performance would be affected .So Water Jet cutting , Underwater plasma cutting